Dow Corning BY 25-337 Silicone Emulsifier

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning BY 25-337 Silicone Emulsifier.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This emulsifier for water-in-oil and water-in-silicone emulsions can be used in a wide range of personal care applications such as skin care, color cosmetics, sun care, hair care, and antiperspirants & deodorants.Dow Corning® BY 25-337 is a crystal clear 50% dispersion of a high molecular weight silicone surfactant (polyoxyethylene/polyoxypropylene copolymer) in Isoparaffin.It can be used to prepare water-in-silicone or mixed oil phases emulsion systems to deliver both non-polar and polar ingredients.It is designed to prepare clear gels such as Dimethicone, Caprylyl Methicone (Dow Corning® FZ-3196) but also with organics such as Isododecane and Isohexadecane.INCI Name: PEG/PPG-19/19 Dimethicone (and) C13-16 Isoparaffin (and) C10-13 IsoparaffinInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.870 g/cc

@Temperature 25.0 °C
0.870 g/cc

@Temperature 77.0 °F
Viscosity Measure 3000 cSt
3000 cSt
Kinetic/Kinematic
Thermal Properties Metric English Comments
Flash Point 88.5 °C
191 °F
Closed cup
Optical Properties Metric English Comments
Refractive Index 1.43
1.43
Descriptive Properties Value Comments
Nonvolatile Content (%) 50