Dow Corning EL-8040 ID Silicone Organic Blend

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning EL-8040 ID Silicone Organic Blend.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dow Corning® EL-8040 ID Silicone Organic Blend is a mixture of high molecular weight silicone elastomer in isododecane. It can be used in color cosmetic, skin care, and sunscreen applications.INCI Name: Isododecane (and) Dimethicone CrosspolymerInformation provided by Dow Corning
Physical Properties Metric English Comments
Viscosity Measure 300000 - 550000 cSt
300000 - 550000 cSt
Kinetic/Kinematic
Descriptive Properties Value Comments
Cyclopentasiloxane Content (%) <1
Cyclotetrasiloxane Content (%) <1
Nonvolatile Content (%) 15.25-16.75