Dow Corning MOLYKOTE® AS-810 GREASE

Category Fluid , Lubricant , Silicone Base
Manufacturer Dow Corning
Trade Name MOLYKOTE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning MOLYKOTE® AS-810 GREASE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone grease with wide service temperature range for starter clutchInformation provided by Dow Corning
Mechanical Properties Metric English Comments
Penetration P(60), 1/10 mm 300
300
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Dropping Point 230 °C
446 °F
Descriptive Properties Value Comments
Color light pink