Dow Corning OS-30

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning OS-30.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.850 g/cc

@Temperature 25.0 °C
0.850 g/cc

@Temperature 77.0 °F
Viscosity 1.3 cP
1.3 cP
dynamic
Vapor Pressure 0.000573 bar

@Temperature 25.0 °C
0.430 torr

@Temperature 77.0 °F
Surface Tension 17.3 dynes/cm
17.3 dynes/cm
Thermal Properties Metric English Comments
Melting Point -68.0 °C
-90.4 °F
Boiling Point 194 °C
381 °F
Flash Point 57.0 °C
135 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 48.0 Month
48.0 Month
Descriptive Properties Value Comments
Appearance clear
Hydrophobic yes
Water Resistant yes