Dow Corning SILASTIC® MDX4-4210 BIOMEDICAL GRADE ELASTOMER WITH CATALYST

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® MDX4-4210 BIOMEDICAL GRADE ELASTOMER WITH CATALYST.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silastic® MDX4-4210 BioMedical Grade Elastomer is designed for use in medical device encapsulating and moldmaking applications where cure is at room temperature or slightly elevated temperatures. Can be used for general prototyping, molding and fabrication of medical device components. Can also be used as a drug matrix for controlled release drug delivery systems.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Elongation at Break 470 %
470 %