Dow Corning SILASTIC® Q7-4840 BIOMEDICAL GRADE ETR ELASTOMER, KIT

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® Q7-4840 BIOMEDICAL GRADE ETR ELASTOMER, KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Tensile Strength, Ultimate 9.45 MPa
1370 psi
Elongation at Break 540 %
540 %
Tear Strength 36.8 kN/m
210 pli