Material Notes:
A blend of a unique silicone elastomer and a volatile silicone fluid for use in a wide range of skincare and topical pharmaceutical delivery applications.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.940 g/cc

@Temperature 25.0 °C
0.940 g/cc

@Temperature 77.0 °F
Viscosity Measure 350000 - 490000 cSt
350000 - 490000 cSt
Kinetic/Kinematic
Descriptive Properties Value Comments
Nonvolatile Content (%) 12-13