Material Notes:
Syl-Off® 1171A Catalyst Emulsion is a 50% solids emulsion of an organotin catalyst in water. Suitable for use with Syl-Off® 1181 Emulsion Coating.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
pH 5.5
5.5
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 50
Appearance liquid
Color milky white