Dow Corning SYL-OFF® 7780 RELEASE MODIFIER

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name SYL-OFF®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SYL-OFF® 7780 RELEASE MODIFIER.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Syl-off® 7780 Release Modifier is a 100% active solids, pre-catalysed, release modifier. High efficiency release modifier suitable for use with Syl-off® brand silicone release coatings.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc

@Temperature 25.0 °C
1.02 g/cc

@Temperature 77.0 °F
Kinematic Viscosity 1000 cSt
1000 cSt
Thermal Properties Metric English Comments
Flash Point 100 °C
212 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Appearance colorless liquid
Color pale yellow
Solvent solventless