Material Notes:
Is chemically equivalent to DOW CORNING® 2-1273 FLUID. This product is an OH end-blocked polydimethylsiloxane, visc. 50-120 cst., OH/Silanol content 2.5%.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity Measure 50 - 120 cSt
50 - 120 cSt
Kinetic/Kinematic
Descriptive Properties Value Comments
Silanol Content (%) 2.5
Users viewing this material also viewed the following: