Material Notes:
Phenyltrichlorosilane fluidInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.312 g/cc
1.312 g/cc
Kinematic Viscosity 1.01 cSt
1.01 cSt
Molecular Weight 211.6 g/mol
211.6 g/mol
Thermal Properties Metric English Comments
Boiling Point 35.0 °C
95.0 °F
Flash Point 79.0 °C
174 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance colorless