Dow Corning Z-6582 SILANE

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning Z-6582 SILANE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hydrophobing and dispersing agentInformation provided by Dow Corning
Physical Properties Metric English Comments
Molecular Weight 206 g/mol
206 g/mol
Descriptive Properties Value Comments
Hydrophobic yes
Purity (%) 100