Dow Nordel® NDR 46140.01 EPDM Hydrocarbon Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Dow Chemical
Trade Name Nordel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Nordel® NDR 46140.01 EPDM Hydrocarbon Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: NDR 46140.01 is a developmental product in granular form that contains carbon black as a partitioning agent. It is a very high molecular weight, amorphous EPDM grade with a fast cure rate. It also offers an excellent combination of:very fast mixing with good dispersion levelexcellent tensile strength and compression set resistance, even at very high loadingIt was designed for highly extended compounds to be used in applications such as extruded profiles, hose and seals.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D297
Volatiles <= 0.40 %
<= 0.40 %
Total Volatiles; DuPont Dow EPRG-21
Mooney Viscosity 140

@Temperature 125 °C
140

@Temperature 257 °F
Polymer (calculated), ML 1 + 4
Descriptive Properties Value Comments
Carbon Black Content (N650) 30 phr
DuPont Dow EPRG-2
ENB 4.9 mass%
ASTM D6047
Ethylene 58 mass%
ASTM D3900
Users viewing this material also viewed the following: