Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Du-Co Ceramics DC-187 Magnesium Oxide

Category Ceramic , Oxide , Magnesium Oxide
Manufacturer Du-Co Ceramics Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Du-Co Ceramics DC-187 Magnesium Oxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
Physical Properties Metric English Comments
Density 2.10 - 2.50 g/cc
0.0759 - 0.0903 lb/in³
Water Absorption 15 - 20 %
15 - 20 %
Porous
Mechanical Properties Metric English Comments
Flexural Strength 10.0 MPa
1450 psi
Compressive Strength 17.0 MPa
2470 psi
Users viewing this material also viewed the following: