DuPont Performance Polymers AquaStik® AQS-2161 Polychloroprene Latex  (discontinued **)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers AquaStik® AQS-2161 Polychloroprene Latex  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Aquastik™ polychloroprene latexes have been designed for the adhesives industry. They provide an environmentally friendly alternative to solvent-borne systems.This grade features post-forming. 59% Solids. Main uses are in adhesives. Initial pH is 12.5. High gel polymer type. Potassium salt of disproportionated rosin acids used as emulsifying agent. Slow crystallization rate.Information provided by DuPont Dow Elastomers.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Latex
1.25 g/cc
0.0452 lb/in³
Polymer
Brookfield Viscosity 27.5 cP
27.5 cP