Material Notes:
Crastin® LW9330 NC010 is a 30% glass fiber reinforced polybutylene terephthalate alloy for injection molding. It has improved surface aesthetics, excellent dimensional stability and low warpage characteristics.Information provided by DuPont Performance Polymers