Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)  (Unverified Data**)

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Unreinforced
Manufacturer DuPont Performance Polymers
Trade Name Delrin®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Delrin® PC691 NC010 Acetal (POM)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nucleated Low Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC690 is a low viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.42 g/cc
0.0513 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 75.0 MPa
10900 psi
ISO 527-1/-2
Elongation at Break 20 %
20 %
Nominal; ISO 527-1/-2
Elongation at Yield 10 %
10 %
ISO 527-1/-2
Tensile Modulus 3.40 GPa
493 ksi
ISO 527-1/-2
Charpy Impact, Notched 0.800 J/cm²
3.81 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Additives Lubricants
Release agent
Delivery Form Pellets
Part Marking Code >POM<
ISO 11469
Processing Injection Moulding
Regional Availability Asia Pacific
Europe
Global
Near East/Africa
North America
South and Central America
Resin Identification POM
ISO 1043