Material Notes:
Delrin® SC699 is a low viscosity acetal homopolymer, lubricated, developed for parts requiring high precision molding in the healthcare industry.Information provided by DuPont Performance Polymers
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength, Yield 63.0 MPa

@Temperature 23.0 °C
9140 psi

@Temperature 73.4 °F
ISO 527
Elongation at Yield 12 %

@Temperature 23.0 °C
12 %

@Temperature 73.4 °F
ISO 527
Tensile Modulus 3.05 GPa

@Temperature 23.0 °C
442 ksi

@Temperature 73.4 °F
ISO 527
Charpy Impact, Notched 0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 178 °C
352 °F
10°C/min; ISO 11357-1/-3
Descriptive Properties Value Comments
Additive Lubricant
Appearance Natural Color
Features Wear Resistance, Good
Forms Pellets
Generic Acetal (POM) Homopolymer
Material Status Current
Part Marking Code >POM-S<
ISO 11469
Processing Method Injection Molding
Product Category Healthcare Resins
Low Wear and Friction Resins
Unreinforced Resins
Region Available - Global Yes
Resin Identification POM-S
ISO 1043
RoHS Compliance Contact Manufacturer
Uses Medical Applications