DuPont Performance Polymers Kalrez® 8575 FFKM Perfluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 8575 FFKM Perfluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Kalrez® Sahara™ 8575 is specially formulated for improved performance in etching, ashing and stripping processes, offers lower cost of ownership with reduced contamination and longer seal life. This white perfluoroelastomer compound utilizes a new proprietary polymer and crosslinking system. It offers reduced weight loss, particle generation and outgassing, as well as improved elastic recovery properties. Kalrez® Sahara™ 8575 exhibits excellent resistance to both oxygen and fluorine plasma as well as chlorinated cleaning gasses (e.g., CIF3). It has excellent vacuum and long-term sealing performance, good mechanical properties and is well-suited for both static and dynamic sealing applications (e.g., gas inlets, chamber lids, slit valve doors, etc.). A maximum continuous service temperature of 300°C is suggested. Ultrapure post-cleaning and packaging is standard for all parts made of Kalrez® Sahara™ 8575.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by DuPont Performance Elastomers.
Mechanical Properties Metric English Comments
Hardness, Shore M 74
74
ASTM D2240, D1414 (O-ring data)
Tensile Strength, Ultimate 12.0 MPa
1740 psi
20 in/min; ASTM D412 (dumbbells)
Elongation at Break 230 %
230 %
20 in/min; ASTM D412 (dumbbells)
100% Modulus 0.00250 GPa
0.363 ksi
20 in/min; ASTM D412 (Dumbbells)
Compression Set 25 %

@Temperature 204 °C
25 %

@Temperature 399 °F
675 hr; ASTM D395B & D 1414 (214 O-rings)
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F