DuPont Performance Polymers Kalrez® 9300 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® 9300 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Kalrez® 9300 perfluoroelastomer parts are a brown product for Dielectric (Oxide) Etch processes. It has been specifically designed for use in applications where the plasma environment is a combination of ions (“physical”) and radicals (“chemical”), i.e., where a balance of “physical” and “chemical” plasma erosion resistance is typically required. Kalrez® 9300 exhibits excellent resistance to oxygen and fluorine-based plasma and etch process chemistry. It also offers very low metals content, excellent thermal stability and mechanical strength, and is well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 300°C is suggested. Ultrapure post-cleaning and packaging is standard for all Kalrez® 9300 parts. Features/Benefits: Low erosion rate and ultra-low particle generation in ion/radical dominant oxygen and fluorine-based plasmas Excellent resistance to etch process chemistry Very low metals content Excellent thermal stability Excellent mechanical strength Suggested Applications Gas inlet/orifice seals Chamber lid seals Isolation valve seals Bonded gate valves/slit valve door seals
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Plied slab; ASTM D2240
Hardness, Shore M 78
78
O-ring; ASTM D1414, ASTM D2240
Tensile Strength at Break 16.57 MPa
2403 psi
ASTM D1414, ASTM D412
Elongation at Break 215 %
215 %
ASTM D1414, ASTM D412
100% Modulus 0.00666 GPa
0.966 ksi
ASTM D1414, ASTM D412
Compression Set 20 %

@Temperature 204 °C,
Time 252000 sec
20 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
37 %

@Temperature 250 °C,
Time 252000 sec
37 %

@Temperature 482 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
DuPont Test Method
Descriptive Properties Value Comments
Color Brown