DuPont Performance Polymers Kalrez® PV8070 Fluoroelastomer

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Kalrez®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Kalrez® PV8070 Fluoroelastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Kalrez® PV8070 perfluoroelastomer parts are a black product for PV cell manufacturing processes requiring high temperature resistance including doping for n-type layer formation (bulk c-Si), diffusion for diselenide thermal implantation (CGIS) and TCS-based thermal CVD for poly-silicon feedstock production. It exhibits outstanding thermal stability and has excellent (low) compression set and outgassing properties. It also offers excellent resistance to both chlorine and fluorine gas as well as other dry process chemistry. Kalrez® PV8070 perfluoroelastomer parts have excellent mechanical strength properties and are well suited for both static and dynamic sealing applications. A maximum continuous service temperature of 325 °C is suggested. Short excursions to higher temperatures may also be possible. Features/Benefits Outstanding thermal stability Excellent (low) compression set and outgassing properties Excellent resistance to dry process chemistry Excellent mechanical strength properties Suggested Applications Chamber lid and door seals Center ring seals and fittings Isolation valve seals Quartz tube seals Substrate handling pads
Mechanical Properties Metric English Comments
Hardness, Shore M 83
83
ASTM D1414, ASTM D2240
Compression Set 9.0 %

@Temperature 204 °C,
Time 252000 sec
9.0 %

@Temperature 399 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
32 %

@Temperature 300 °C,
Time 252000 sec
32 %

@Temperature 572 °F,
Time 70.0 hour
ASTM D1414 and ASTM D395B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 325 °C
617 °F
DuPont Test Method
Descriptive Properties Value Comments
Color Black