DuPont Performance Polymers Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Chlorosulfonated Polyethylene Rubber
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name Neoprene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers Neoprene 750 Copolymer of chloroprene and 2,3,dichloro-1,3,-butadiene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DuPont™ Neoprene 750 is an aqueous colloidal dispersion of a crystallization-resistant Neoprene. Its crystallization resistance is similar to that of DuPont™ Neoprene WRT. Neoprene 750 is anionic and is extremely stable with respect to shelf and heat aging. It immediately forms strong, highly extensible films when coagulated.Main Features Outstanding wet gels elongation and wet gel tensile strength render Neoprene 750 useful in dipped goods applications resist gel cracking either alone or in blends with other Neoprene liquid dispersion products such as DuPont™ Neoprene 571, or DuPont™ Neoprene 842A. The low modulus of Neoprene 750 allows manufacture of very flexible products or dipped goods. Neoprene 750 compounds without filler loading duplicate the lower stress/strain curve of similarly natural rubber latex products. The high resistance to crystallization of Neoprene 750 allows it to maintain low modulus at relatively low temperatures regardless of the state of cure. Suggested End Uses Dipped goods Contact bond adhesives Cord adhesives Construction adhesives
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Liquid Dispersion
1.25 g/cc
1.25 g/cc
Polymer
Solids Content 50 %
50 %
pH >= 12
>= 12
Descriptive Properties Value Comments
Color Off-white
Compounding Stability Good
Emulsifying Agent Potassium salts
Freeze/Thaw Stability Not stable
Mechanical Stability Good
Storage Stability Good