Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Performance Polymers VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Performance Polymers (Former DuPont Elastomers)
Trade Name VTR
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Performance Polymers VTR GLT Peroxide Cured Fluoroelastomer (FKM) Formulation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FormulationViton® VTR-8500
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Tensile Strength, Ultimate 17.6 MPa
2550 psi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Elongation at Break 181 %
181 %
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Modulus of Elasticity 0.000600 GPa
0.0870 ksi
10% Modulus, Cured 7 min at 177°C and Post Cured 16 hr at 232°C
100% Modulus 0.00590 GPa
0.856 ksi
Cured 7 min at 177°C and Post Cured 16 hr at 232°C
Compression Set 16 %

@Temperature 200 °C
16 %

@Temperature 392 °F
Method B, O-rings 22 hr at 200°C (Cured 7 min at 177°C and Post Cured 16 hr at 232°C)
Thermal Properties Metric English Comments
Brittleness Temperature -30.6 °C
-23.1 °F
TR-10
Glass Transition Temp, Tg -30.7 °C
-23.3 °F
DSC