DuPont™ Tedlar® SP TTR10SH9 Clear Polyvinyl Fluoride Film

Category Polymer , Film , Thermoplastic , Fluoropolymer
Manufacturer DuPont
Trade Name Tedlar® SP
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont™ Tedlar® SP TTR10SH9 Clear Polyvinyl Fluoride Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tedlar® SP polyvinyl fluoride film is designed to provide excellent conformability to substrates while maintaining the good durability, color stability, chemical resistance, and ease of cleaning expected of PVF film. Tedlar® SP also offers custom color capability not previously available in PVF film. Tedlar® SP is an unoriented film. It possesses high elongation and moderate yield stress. After lamination using conventional means, it can be easily embossed and will maintain high pattern definition. Tedlar® SP can also be subjected to high levels of forming without significant recovery stresses.Information provided by DuPont.
Mechanical Properties Metric English Comments
Tensile Strength 34.0 MPa
4930 psi
ASTM D882-80, Method A - 100%
Film Elongation at Break, MD 250 %

@Temperature 20.0 °C
250 %

@Temperature 68.0 °F
375 %

@Temperature 50.0 °C
375 %

@Temperature 122 °F
Film Elongation at Break, TD 260 %

@Temperature 20.0 °C
260 %

@Temperature 68.0 °F
350 %

@Temperature 50.0 °C
350 %

@Temperature 122 °F
Film Tensile Strength at Break, TD 13.1 MPa

@Temperature 100 °C
1900 psi

@Temperature 212 °F
22.1 MPa

@Temperature 75.0 °C
3200 psi

@Temperature 167 °F
31.7 MPa

@Temperature 50.0 °C
4600 psi

@Temperature 122 °F
41.4 MPa

@Temperature 20.0 °C
6000 psi

@Temperature 68.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified