Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® 965 Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® 965 is a slightly hazy film with internal UV blocker. It is pretreated on one surface to promote adhesion to many solvent systems. It has a superb web handleability.Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 96.5 MPa
14000 psi
ASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa
14000 psi
ASTM D882A
Film Elongation at Break, MD 180 %
180 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.25
0.25
A-B, untreated to treated; ASTM D1894
Film Tensile Strength at Break, MD 165 MPa
24000 psi
ASTM D882A
Film Tensile Strength at Break, TD 207 MPa
30000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 2.0 %

@Temperature 190 °C,
Time 300 sec
2.0 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD 2.3 %

@Temperature 190 °C,
Time 300 sec
2.3 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Optical Density 0.55
0.55
UV OD with Wratten 18A Filte
Haze 4.0 %
4.0 %
ASTM D1003
Users viewing this material also viewed the following: