DuPont Teijin Films Melinex® HS2 Polyester Film

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Melinex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Melinex® HS2 Polyester Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melinex® HS2 is a low TD shrinkage, low neckdown polyester film with excellent handling properties. It is ideal for the hot stamping marketInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 107 MPa
15500 psi
ASTM D882A
Film Tensile Strength at Yield, TD 96.5 MPa
14000 psi
ASTM D882A
Film Elongation at Break, MD 105 %
105 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Coefficient of Friction, Dynamic 0.40
0.40
A-B; ASTM D1894
Film Tensile Strength at Break, MD 241 MPa
35000 psi
ASTM D882A
Film Tensile Strength at Break, TD 238 MPa
34500 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 3.6 %

@Temperature 190 °C,
Time 300 sec
3.6 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Shrinkage, TD -0.200 %

@Temperature 190 °C,
Time 300 sec
-0.200 %

@Temperature 374 °F,
Time 0.0833 hour
Unrestrained
Optical Properties Metric English Comments
Haze 4.0 %

@Thickness 0.0122 mm
4.0 %

@Thickness 0.000480 in
ASTM D1003
4.8 %

@Thickness 0.0152 mm
4.8 %

@Thickness 0.000600 in
ASTM D1003
5.7 %

@Thickness 0.0191 mm
5.7 %

@Thickness 0.000750 in
ASTM D1003
6.7 %

@Thickness 0.0234 mm
6.7 %

@Thickness 0.000920 in
ASTM D1003
Descriptive Properties Value Comments
Yield (nominal) 14000 in2/lb
92 Gauge
26500 in2/lb
75 Gauge
33000 in2/lb
60 Gauge
42200 in2/lb
48 Gauge