DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 80 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® G2 Polyester Film, 80 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® G2 is a polyester film which has high clarity and good slip characteristics.Teijin® Tetoron® G2 is available in the following variations:G2: Non-pretreatedG2N: Adhesion Pretreated (one side)G2C: Corona Treated (one side)G2Z: Release Pretreated (one side) Typical Applications: Teijin® Tetoron® G2 is suitable for applications where low haze and good handling are desired product qualities. Intended applications include:LabelsRelease FilmsHologramsDry Film Resist (DFR)Information provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 150 %
150 %
ASTM D882A
Film Elongation at Break, TD 100 %
100 %
ASTM D882A
Film Tensile Strength at Break, MD 254.93 MPa
36975 psi
ASTM D882A
Film Tensile Strength at Break, TD 303.9 MPa
44080 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 1.7 %

@Temperature 150 °C,
Time 1800 sec
1.7 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.90 %

@Temperature 150 °C,
Time 1800 sec
0.90 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 2.2 %
2.2 %
ASTM D1003