Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 400 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® HS Polyester Film, 400 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® HS is a very clear polyester film. It is available in a wide range of thicknesses.Typical Applications: OHP SheetLabelsITOLaminated CardsWindow FilmInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 190 %
190 %
ASTM D882A
Film Elongation at Break, TD 130 %
130 %
ASTM D882A
Coefficient of Friction, Dynamic 0.25
0.25
ASTM D1894
Coefficient of Friction, Static 0.28
0.28
ASTM D1894
Film Tensile Strength at Break, MD 196.95 MPa
28565 psi
ASTM D882A
Film Tensile Strength at Break, TD 241.9 MPa
35090 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.70 %

@Temperature 150 °C,
Time 1800 sec
0.70 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.20 %

@Temperature 150 °C,
Time 1800 sec
0.20 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ASTM D1003