Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 300 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® HSL Polyester Film, 300 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® HSL is a low shrinkage polyester film with well balanced physical, chemical and optical properties. In addition to the standard, non-pretreated, Teijin® Tetoron® HSL film, the following variations are available: HLE: Slip and adhesion treated - one side and HLW: Slip and adhesion treated - both sidesTypical Applications: Teijin® Tetoron® HSL film is suitable for many optical and imaging applications where low thermal shrinkage and low haze are important characteristics. It is recommended for:ImagingMembrane Touch Switches (MTS)OHPLayout BaseGraphic ArtsDecorative LaminatesLabelsInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 200 %
200 %
ASTM D882A
Film Elongation at Break, TD 130 %
130 %
ASTM D882A
Coefficient of Friction, Dynamic 0.30
0.30
ASTM D1894
Coefficient of Friction, Static 0.30
0.30
ASTM D1894
Film Tensile Strength at Break, MD 205.9 MPa
29870 psi
ASTM D882A
Film Tensile Strength at Break, TD 244.94 MPa
35525 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.40 %

@Temperature 100 °C,
Time 1800 sec
0.40 %

@Temperature 212 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD -0.100 %

@Temperature 150 °C,
Time 1800 sec
-0.100 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Optical Properties Metric English Comments
Haze 1.5 %
1.5 %
ASTM D1003
Users viewing this material also viewed the following: