Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 500 Gauge

Category Polymer , Film , Thermoplastic , Polyester, TP , Polyester Film
Manufacturer DuPont Teijin Films (DTF)
Trade Name Teijin® Tetoron®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Teijin Films Teijin® Tetoron® SL Polyester Film, 500 Gauge.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Teijin® Tetoron® SL is a low shrinkage version of Teijin® Tetoron® type S polyester film. In addition to having the well balanced physical, chemical and electrical properties of type S film, Teijin® Tetoron® SL has achieved lower thermal shrinkage characteristicsTypical Applications: Teijin® Tetoron® SL film is suitable for use in many industrial applications where lower thermal shrinkage is an important property, such as:Flexible Printed CircuitsMembrane Touch Switches (MTS)Flat CableInformation provided by DuPont.
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 180 %
180 %
ASTM D882A
Film Elongation at Break, TD 130 %
130 %
ASTM D882A
Film Tensile Strength at Break, MD 200 MPa
29000 psi
ASTM D882A
Film Tensile Strength at Break, TD 221 MPa
32000 psi
ASTM D882A
Thermal Properties Metric English Comments
Shrinkage, MD 0.20 %

@Temperature 150 °C,
Time 1800 sec
0.20 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Shrinkage, TD 0.00 %

@Temperature 150 °C,
Time 1800 sec
0.00 %

@Temperature 302 °F,
Time 0.500 hour
Unrestrained
Users viewing this material also viewed the following: