Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DuPont Vamac® DP 3.5 phr Peroxide Test Compound

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Vamac®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Vamac® DP 3.5 phr Peroxide Test Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temperature resistanceGood compression set resistanceGood low temperature flexibilityUnlike Vamac® terpolymers, Vamac® DP dipolymer can be processed without a post cure.Form: Bale size is nominally:560 mm x 370 mm by 165 mmInformation provided by DuPont.
Physical Properties Metric English Comments
Mooney Viscosity 51

@Temperature 100 °C
51

@Temperature 212 °F
ML(1+4), mu
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
Cured 10 minutes at 180°C
Tensile Strength, Ultimate 16.1 MPa
2340 psi
Cured 10 minutes at 180°C
Elongation at Break 254 %
254 %
Cured 10 minutes at 180°C
100% Modulus 0.00580 GPa
0.841 ksi
Cured 10 minutes at 180°C
Compression Set 52 %
52 %
168 hrs at 150°C
Descriptive Properties Value Comments
Armeen® 18D 0.5 phr
HVA® #2 coagent 2 phr
Mooney Scorch at 135°C, Minimum Viscosity 12.8
Mooney units
Mooney Scorch at 135°C, t10 19 metric minutes
Time for 10 unit rise
Mooney Scorch at 135°C, t3 11.5 metric minutes
Time for 3 unit rise
N550 Black 55 phr
Naugard® 445 antioxidant 1 phr
Stearic Acid 0.5 phr
Vamac® DP 100 phr
Vanfre® VAM 1.25 phr
Vulcup® 40LE peroxide 3.5 phr
Users viewing this material also viewed the following: