DuPont Vamac® G Ethylene Methylacrylate Terpolymer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer DuPont Packaging and Industrial Polymers
Trade Name Vamac®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DuPont Vamac® G Ethylene Methylacrylate Terpolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vamac® G is a terpolymer of ethylene, methylacrylate, and a cure site monomer cured using an amine-based vulcanization system. This gum elastomer includes a small amount of processing aid. It has excellent storage stability.Vamac® G has excellent high-temperature durability and oil resistance with service lubricants, coupled with good low-temperature flexibility. Compounds of Vamac® G are typically rated at 175°C (347°F) for heat resistance, with oil swell values around 50% in ASTM No. 3 oil. These properties of Vamac® G make it well suited for a wide range of automotive applications, including powertrain seals and gaskets, rocker cover and piston seals, oil coolant hoses, power steering hoses, turbocharger hoses, crankcase ventilating tubes, coverings for fuel and coolant hoses, O-rings, grommets and spark plug boots.Vamac® G is an excellent vibration damping material that is uniquely insensitive to temperature over a range of -30°C (-22°F) to 160°C (320°F). Compounds of Vamac® G are suitable for use in torsional dampers and isolator pads. Vamac® G is a halogen-free polymer and does not decompose to give off corrosive gases when exposed to flame. It is used for flame-retardant, low-smoke, nonhalogen wire and cable jackets and in nonhalogen, low-smoke flooring. Vamac® G is well suited for injection, transfer and compression molding, and is easily extruded.Form: Bale size is nominally:560 mm x 370 mm by 165 mmInformation provided by DuPont.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Nominal
Mooney Viscosity 14 - 19

@Temperature 100 °C
14 - 19

@Temperature 212 °F
ML(1+4); ASTM D1646
Collected Volatile Condensable Material <= 0.70 %
<= 0.70 %
DuPont Test MP 726-1
Descriptive Properties Value Comments
Color Clear
Visual inspection
Odor Mild acrylic