Dymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic Bonder

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic Bonder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-20275 Coil Terminating, Tamper proofing and Structural Electronic BonderExcellent adhesion to plastics, glass, metal and porous materials, cures with UV or visible light. Cure Type: UV, Visible, Activator or Heat
Physical Properties Metric English Comments
Viscosity 2500 cP
2500 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.9 MPa
2600 psi
Processing Properties Metric English Comments
Cure Time <= 0.0167 min
<= 0.000278 hour
Descriptive Properties Value Comments
Cure Depth 0.5 in.