EMS-Griltech Grilon® KA 115 White CoPA Fiber Count 2.2

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® KA 115 White CoPA Fiber Count 2.2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON KA 115 is the low melting homo component fusible adhesive fiber.Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 2.20 dtex
1.98 denier
Processing Properties Metric English Comments
Melt Temperature 110 - 120 °C
230 - 248 °F
Descriptive Properties Value Comments
Color Raw White
Luster Bright
Staple Length 38 mm