EMS-Griltech Grilon® TM 5000 White Nylon 6 Fiber, Medium Fiber Count

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6 Fiber
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® TM 5000 White Nylon 6 Fiber, Medium Fiber Count.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON TM 5000 is a standard product for the manufacturing of press felts. This is a technical fiber with medium-set fixation. This fiber is also available as TM 5010 (low crimp) and TM 5020 (high crimp).Data provided by EMS-Griltech.
Physical Properties Metric English Comments
Fiber Count 6.70 - 11.0 dtex
6.03 - 9.90 denier
Descriptive Properties Value Comments
Color Raw White
Crimp Standard
Luster Bright
Staple Length vario 3 mm