EMS-Griltech Grilon® XA 930 Modified Nylon Monofilament (Medium-Set)

Category Polymer , Thermoplastic , Nylon
Manufacturer EMS-Griltech
Trade Name Grilon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF EMS-Griltech Grilon® XA 930 Modified Nylon Monofilament (Medium-Set).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: GRILON XA 930 is a Modified Nylon based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Filament Diameter 200 - 350 µm
200 - 350 µm
Mechanical Properties Metric English Comments
Elongation at Break 35 - 55 %
35 - 55 %
Tenacity 0.384 - 0.473 N/tex
4.35 - 5.36 g/denier
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
Shrinkage 6.00 - 8.00 %

@Temperature 180 °C
6.00 - 8.00 %

@Temperature 356 °F
Thermo Shrinkage
Descriptive Properties Value Comments
Heat Setting Medium-Set