Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eifeler Coatings Technology SUCASLIDE® DLC coating

Category Carbon , Diamond , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name SUCASLIDE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology SUCASLIDE® DLC coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Further significant improvement of the slide characteristics with respect to traditional PVD layers (also with minimal lubrication a significant improvement results) decrease of adhesion and both friction partners are protected.Information provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 0.300 - 0.700 microns
0.0118 - 0.0276 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 1800 - 2000
1800 - 2000
Coefficient of Friction 0.050 - 0.10
0.050 - 0.10
cemented carbide
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C
752 °F
Descriptive Properties Value Comments
Color black