Material Notes:
Key Characteristics: high warm hardness, very high oxidation resistance, high protection against abrasive wearPrimary Applications: warm forming, hot forging, and die casting; coating for milling with carbide, cermet and high speed steel tools; machining under dry conditions; available with in-situ Duplex treatmentInformation provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 3.00 - 5.00 microns
0.118 - 0.197 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 3000 - 3600
3000 - 3600
Coefficient of Friction 0.60
0.60
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 900 °C
1650 °F
Descriptive Properties Value Comments
Color dark gray