Eifeler Coatings Technology WC/C PVD Coating

Category Ceramic , Carbide , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Eifeler Coatings Technology
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eifeler Coatings Technology WC/C PVD Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Characteristics: high lubricity, low tendency for adhesive wearPrimary Applications: on top of hard coatings for reduction of friction; precision components: automotive, aerospace, medicalInformation provided by Eifeler Coatings Technology
Physical Properties Metric English Comments
Thickness 1.00 - 4.00 microns
0.0394 - 0.157 mil
Mechanical Properties Metric English Comments
Vickers Microhardness 1000 - 2200
1000 - 2200
Coefficient of Friction 0.20 - 0.25
0.20 - 0.25
dry, steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 400 °C
752 °F
Descriptive Properties Value Comments
Color black