Densified laminated woodInformation provided by elisto
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Water Absorption >= 5.0 %
>= 5.0 %
Mechanical Properties Metric English Comments
Flexural Strength 90.0 MPa

@Temperature 23.0 °C
13100 psi

@Temperature 73.4 °F
Flexural Modulus 8.00 GPa
1160 ksi
Compressive Strength 140 MPa

@Temperature 23.0 °C
20300 psi

@Temperature 73.4 °F
Descriptive Properties Value Comments
Application Temperature (°C) 110