Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK) , Polyetheretherketone, PEEK, PTFE-Filled
Manufacturer Ensinger
Trade Name Tecapeek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecapeek® XP-95 Compression Molded PEEK Compound, 15% PTFE Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in lower amounts of scrap, uniform physical properties and fewer molded-in stresses.TECAPEEK is a high-perfomance engineering thermoplastic. This semi-crystalline material has a balance of high temperature mechanical properties, chemical and steam resistance, superior wear properties and processability which makes it unique.Applications Include:Bearings and BushingsDown-hole instrumentationWear RingsBall Valve SeatsElectrical ComponentsBack-up and V-RingsPiston Rings and Rider BandsInformation provided by Ensinger Special Polymers, Inc.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Filler Content 15 %
15 %
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Hardness, Shore D 88
88
ASTM D2240
Tensile Strength 79.3 MPa
11500 psi
ASTM D638
Elongation at Break 4.3 %
4.3 %
ASTM D638
5.0 %
5.0 %
Flexural Strain; ASTM D790
Tensile Modulus 3.79 GPa
550 ksi
ASTM D638
Flexural Strength 134 MPa
19500 psi
ASTM D790
Flexural Modulus 4.34 GPa
630 ksi
ASTM D790
Compressive Strength <= 221 MPa
<= 32000 psi
ASTM D695
Izod Impact, Notched 0.352 J/cm
0.660 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.080
0.080
ASTM D3702
Coefficient of Friction, Static 0.17
0.17
ASTM D3702
Thermal Properties Metric English Comments
Melting Point 343 °C
649 °F
DSC
Descriptive Properties Value Comments
Color Tan