Material Notes:
This product is intended for injection molding applications such as automotive, appliance, lawn and garden, consumer products and industrial application. This product offers high impact properties at both room temperature and cold temperatures.Information provided by Entec
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Modulus, 1% Secant 966 MPa
140000 psi
ASTM D790
Izod Impact, Notched >= 5.35 J/cm

@Thickness 3.17 mm
>= 10.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ASTM D648
Users viewing this material also viewed the following: