Esstech X-743-0000 Ethoxylated Bis Phenol A Dimethacrylate, C43H64O14

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Esstech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-743-0000 Ethoxylated Bis Phenol A Dimethacrylate, C43H64O14.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This form of EBPADMA has 10 units of ethoxylation. Polymerization of this material results in a rigid polymer with high degree of conversion. Listed on the Toxic Substance Control Act List. CAS # 41637-38-1.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Viscosity 410 cP

@Temperature 25.0 °C
410 cP

@Temperature 77.0 °F
Molecular Weight 805 g/mol
805 g/mol
Optical Properties Metric English Comments
Refractive Index 1.5112
1.5112