Esstech X-851-0000 Urethane Dimethacrylate IPDI, C24H38N2O8

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Esstech
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Esstech X-851-0000 Urethane Dimethacrylate IPDI, C24H38N2O8.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
UDMA-IPDI has a higher viscosity than our X-850-0000, urethane dimethacrylate. The high molecular weight of X-851-0000 results in lower polymerization shrinkage when cured.Information provided by ESSTECH, Inc.
Physical Properties Metric English Comments
Molecular Weight 482.57 g/mol
482.57 g/mol
Optical Properties Metric English Comments
Refractive Index 1.4938
1.4938