Eurofoam Porocell 251 BG NBR/PVC Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell 251 BG NBR/PVC Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.150 - 0.190 g/cc
0.00542 - 0.00686 lb/in³
ISO 845-88
Water Absorption <= 1.5 %
<= 1.5 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 55 - 65
55 - 65
ASTM D 2240
Tensile Strength 0.320 MPa
46.4 psi
ASTM D 412
Elongation at Break >= 220 %
>= 220 %
ASTM D 412
Compressive Yield Strength 0.0670 MPa

@Strain 25.0 %
9.72 psi

@Strain 25.0 %
ASTM 1056/85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
ASTM D 3575
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
ASTM D 3575
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black, White
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Vulcanization Peroxide