Eurofoam Porocell POR 304 B-OPC EPDM Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell POR 304 B-OPC EPDM Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0850 - 0.115 g/cc
0.00307 - 0.00415 lb/in³
ISO 845-88
Mechanical Properties Metric English Comments
Hardness, Shore OO 7.0 - 13
7.0 - 13
ASTM D 2240
Tensile Strength 0.100 MPa
14.5 psi
ASTM D 412
Elongation at Break >= 100 %
>= 100 %
ASTM D 412
Compressive Yield Strength 0.00230 MPa

@Strain 25.0 %
0.334 psi

@Strain 25.0 %
ASTM 1056/85
0.00380 MPa

@Strain 50.0 %
0.551 psi

@Strain 50.0 %
ASTM 1056/85
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Shrinkage <= 1.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 1.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Open
Color Black
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Vulcanization Sulfur