Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Porocell POR 304 CM-BI EPDM Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell POR 304 CM-BI EPDM Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.100 - 0.140 g/cc
0.00361 - 0.00506 lb/in³
ISO 845-88
Water Absorption <= 5.0 %
<= 5.0 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 45 - 55
45 - 55
ASTM D 2240
Tensile Strength 0.450 MPa
65.3 psi
ASTM D 412
Elongation at Break >= 150 %
>= 150 %
ASTM D 412
Compressive Yield Strength 0.0350 MPa

@Strain 25.0 %
5.08 psi

@Strain 25.0 %
ASTM 1056/85
0.0700 MPa

@Strain 50.0 %
10.2 psi

@Strain 50.0 %
ASTM 1056/85
Tear Strength 0.280 kN/m
1.60 pli
ASTM D 624
Compression Set 12 %

@Strain 25.0 %
12 %

@Strain 25.0 %
ASTM D 395
18 %

@Strain 50.0 %
18 %

@Strain 50.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 95.0 °C
203 °F
ASTM D 3575
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color White
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Vulcanization Peroxide