Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Bicor® 120 AB-X OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor® 120 AB-X OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor AB-X is a two-side coated, sealable OPP film designed for general use in many applications, including overwrap, horizontal and vertical packaging. This film is suitable as an unsupported web or in a lamination. It can be surface printed, reverse printed, or used unprinted.Availability: Latin America, North America and South AmericaKey Features:Outstanding optical propertiesRobust machinablityLow and consistent COFExcellent hot slipExcellent stiffnessExcellent flavor and aroma barrierExcellent hot tack and seal strengthVery broad seal rangeFeatures:Acrylic CoatedFlavor & Aroma BarrierIn Lamination Lap SealableApplications:Biscuits/Cookie/CrackersBox OverwrapConfectionery, GumConfectionery, SugarPaper Ream wrapTobaccoUses:Box Overwrap Flexible PackagingHFF Flexible PackagingPre-made Bags - Flexible PackagingTobacco Overwrap Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 5.00 g/m²/day
0.322 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Thickness 30.5 microns
1.20 mil
Nominal; ExxonMobil Method
Coating Weight 27.0 g/m²
16.9 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.23
0.23
ExxonMobil Method
Film Tensile Strength at Break, MD 117 MPa
17000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 228 MPa
33000 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 5.0 %
5.0 %
at 275°F; ExxonMobil Method
Shrinkage, TD 3.5 %
3.5 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.7 %
1.7 %
ExxonMobil Method
Gloss 89 %
89 %
45º; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 178°F
200g/in
Crimp Seal Strength 600 g/in
260°F, 20psi, 3/4sec
Yield 25400 in2/lb