Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Bicor® 310 AB OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor® 310 AB OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor AB is a two-side acrylic coated, sealable OPP film designed for general use in applications, including overwrap, horizontal, and vertical packaging. This film is suitable as an unsupported web or lamination. It can be surface printed, reverse printed, or sued unprinted.Availability: Latin America, North America and South AmericaKey Features:Outstanding optical propertiesRobust machinablityLow and consistent COFExcellent hot slipExcellent flavor and aroma barrierPrintable on both sidesFeatures:Acrylic CoatedFlavor & Aroma BarrierIn Lamination Lap SealableApplications:Biscuits/Cookie/CrackersBox OverwrapConfectionery, GumConfectionery, SugarTobaccoUses:Box Overwrap Flexible PackagingHFF Flexible PackagingPre-made Bags - Flexible PackagingTobacco Overwrap Flexible PackagingVFFS Flexible PackagingProcessing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 5.70 g/m²/day
0.367 g/100 in²/day
38°C, 90% RH; ExxonMobil Method
Thickness 25.4 microns
1.00 mil
Nominal; ExxonMobil Method
Coating Weight 22.2 g/m²
13.9 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.24
0.24
ExxonMobil Method
Film Tensile Strength at Break, MD 137 MPa
19900 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 236 MPa
34200 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Thermal Properties Metric English Comments
Shrinkage, MD 4.5 %
4.5 %
at 275°F; ExxonMobil Method
Shrinkage, TD 3.5 %
3.5 %
at 275°F; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.7 %
1.7 %
ExxonMobil Method
Gloss 87 %
87 %
45º; ExxonMobil Method
Descriptive Properties Value Comments
Crimp Seal MST 205°F
Crimp Seal Strength 560, g/in
260°F, 20psi, 3/4sec
Yield 31000 in2/lb
Users viewing this material also viewed the following: