Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Bicor® 84 AOH OPP Film

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Exxon Chemical
Trade Name Bicor®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Bicor® 84 AOH OPP Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Bicor AOH is a two-side coating OPP film designed for high oxygen barrier laminations. AOH is designed to be used as the outer web in gas-flush applications for dry products.Availability: Latin America, North America and South AmericaKey Features:Excellent optical properties, non-yellowingGood barrier performanceOutstanding flavor and aroma barrierPVOH surface is receptive to water-based or solvent based inks and adhesivesRequires priming for extrusion laminationsFeatures:Acrylic CoatedFlavor & Aroma BarrierGas BarrierOxygen BarrierPVOH CoatedApplications:Crips and SnacksUses:VFFS Flexible PackagingProcessing Method: Inner WEb Adhesive Lamination, Out Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing and Water-based Flexographic Printing Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Water Vapor Transmission 5.70 g/m²/day

@Temperature 37.8 °C
0.367 g/100 in²/day

@Temperature 100 °F
90% RH
Oxygen Transmission Rate 0.310 cc/m²/day

@Temperature 22.8 °C
0.0200 cc/100 in²/day

@Temperature 73.0 °F
0.0% RH; ExxonMobil Method
Thickness 21.3 microns
0.840 mil
Nominal; ExxonMobil Method
Coating Weight 19.4 g/m²
12.1 lb/ream
ExxonMobil Method
Mechanical Properties Metric English Comments
Coefficient of Friction 0.26
0.26
Acrylic/Acrylic; ExxonMobil Method
Film Tensile Strength at Break, MD 121 MPa
17500 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 224 MPa
32500 psi
20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ExxonMobil Method
Gloss 95 %
95 %
45º, Acrylic Surface; ExxonMobil Method
Descriptive Properties Value Comments
Yield 35600 in2/lb